library : gallery of defects :: mill defects

Numerous processing flaws are routinely discovered during the inspection of new sucker rods and couplings.  Bar rolling flaws, thread rolling flaws, forging flaws, surface finish flaws, and dimensional tolerance noncompliance can affect the performance capabilities of new rods and couplings.

 

 

 

‹ SUCKER ROD INSPECTION & RECLAMATION SERVICES ›
9009 N. County Rd. West • Odessa, TX 79764 • Tel: (432) 367-4149 • Fax: (432) 367-7015